表1 各种金属纳米颗粒在纤维素酶/漆酶固定化中的应用
Table 1 Application of MNPs on cellulose or laccase immobilization
序号纳米材料固定/结合模式条件参数
1Fe3O4 NPs [68]戊二醛表面修饰共价结合T=60℃, pH=4.5
2Fe3O4 NPs [69]通过半胱氨酸基团的表面功能化卵清蛋白结合T =80℃, pH=4.5
3Fe3O4@SiO2[70]物理吸附T =70℃, pH=4.0
4Fe3O4 NPs @SiO2[71]APTES共价结合T =25℃, pH=4
5Fe3O4 NPs @SiO2[72]甲基丙烯酸缩水甘油酯表面功能化共价结合T =50℃, pH=5.0
6Fe3O4@SiO2@KIT-6NPs[54]APTES共价结合T =35℃, pH=4.5
7Fe3O4 NPs /壳聚糖[73]戊二醛表面修饰共价结合T =60℃, pH=5.5
8Fe3O4 NPs/壳聚糖[74]戊二醛表面修饰共价结合T =60℃, pH=5.0
9Cu/Fe3O4 NPs[75]APTES共价结合T =80℃, pH=5
10Cu2+ modified Fe3O4-NH2NPs[76]亲和吸附T =35℃, pH=4.5
11Fe3O4@Au NPs[67]通过聚乙二醇和L-天门冬氨酸共价结合T =50℃, pH=4.8
12Fe2O3 NPs[77]戊二醛表面修饰共价结合T =50℃, pH=4.8
13CoFe2O4 NPs [78]基于EDS & NHS的戊二醛结合T =50℃, pH=5.0
14MnO2 NPs [46]戊二醛表面改性卵圆结合T =70℃, pH=5.0