• REACTION KINETICS, CATALYSIS AND…… • Previous Articles     Next Articles

NO-3 and HSO-3 Induced Corrosion of Simulated Archaeological Iron in Humid-Acid Atmosphere)

CAOXia; XUChunchun   

  1. College of Materials Science and Engineering, Beijing University of Chemical Technology, Beijing 100029, China
  • Received:1900-01-01 Revised:1900-01-01 Online:2005-10-28 Published:2005-10-28
  • Contact: CAO Xia

潮湿大气中NO-3和HSO-3对模拟铸铁文物的腐蚀研究

曹霞;许淳淳   

  1. College of Materials Science and Engineering, Beijing University of Chemical Technology, Beijing 100029, China
  • 通讯作者: 曹霞

Abstract: NO3^- and HSO3^- induced corrosion of simulated archaeological iron in humid-acid atmosphere was studied by using periodic wet-dry tests. Surface tension tests, electrochemical impedance measurement, stereoscopic microscopy and energy dispersive atomic X-ray analysis (EDAX) were used to investigate the corrosion processes and products. The results of mass loss measurement showed that the corrosion kinetics can be approximately described by △W = A At^B. With the addition of NO3^-, the value of B increases. NO3^- acts as an inhibitor in the HSO3^- bearing pollutant during the corrosion process. Both the electrochemical impedance measurement and surface tension test confirmed the result of mass loss measurement. In addition, we found that the attack of anions to the metal at the initial corrosion stage was in good agreement with their surface activity.

Key words: corrosion, simulated archaeological iron, corrosion rate, NO3^-, HSO3^-

摘要: NO3^- and HSO3^- induced corrosion of simulated archaeological iron in humid-acid atmosphere was studied by using periodic wet-dry tests. Surface tension tests, electrochemical impedance measurement, stereoscopic microscopy and energy dispersive atomic X-ray analysis (EDAX) were used to investigate the corrosion processes and products. The results of mass loss measurement showed that the corrosion kinetics can be approximately described by △W = A At^B. With the addition of NO3^-, the value of B increases. NO3^- acts as an inhibitor in the HSO3^- bearing pollutant during the corrosion process. Both the electrochemical impedance measurement and surface tension test confirmed the result of mass loss measurement. In addition, we found that the attack of anions to the metal at the initial corrosion stage was in good agreement with their surface activity.

关键词: 潮湿大气;NO3^- HSO3^- 铸铁文物;模拟;腐蚀速率