[1] |
Du Zhongqiang(杜中强).Application of the new hydrogen reformer [J].Petro-chemical Equipment Technology(石油化工设备技术),2005, 26(2):40-41
|
[2] |
Wang W Z, Xuan F Z, Wang Z D, Wang B, LiuJ C. Effect of overheating temperature on the microstructure and creep behavior of HP40Nb alloy[J].Mater.Des.,2011,32: 4010-4016
|
[3] |
Chris M, Clement I, John D. Failure analysis and creep remaining life of hydrogen reformer outlet pigtail tubes [J].Eng.Fail.Anal., 2008, 15:1076-1087
|
[4] |
Shipley D G. Creep damage in reformer tubes[J]. Int. J. Press. Ves. Piping., 1983, 14:21-34
|
[5] |
Project report No. CIEP/2006/SSP9302[R].National Metallurgical Laboratory, Jamshedpur, India, 2006
|
[6] |
Baldev Raj, et al. Pressure Vessels and Piping:Manufacturing and Performance [M]. Oxford: Alpha Science International Ltd., 2009
|
[7] |
Dehmolaei R, Shamanian M, Kermanpur A. Improving weld ability of aged 25Cr-35Ni heat resistant steel/alloy 800 dissimilar welds [J]. Sci. Technol. Weld. Joining.,2007, 12:586-592
|
[8] |
Project report No. CIEP/SSP/2001/0115[R]. National Metallurgical Laboratory, Jamshedpur, India, 2001
|
[9] |
Project report No. CIEP/SSP/2003/0141[R].National Metallurgical Laboratory, Jamshedpur, India 2003
|
[10] |
Report No.CIEP/SSP/1999/077[R].National Metallurgical Laboratory, Jamshedpur, India, 2000
|
[11] |
Tawancy H M, Ul Hamid A, Mohammed A I, Abbas N M. Failure analysis of catalytic steam reformer tubes[J]. Anti. Corros. Method. Mater., 2005, 52:337-339
|
[12] |
de Almeida L H, Ribeiro A F, May I L. Microstructural characterization of modified 25Cr-35Ni centrifugally cast steel furnace tubes [J].Mater. Charact., 2003, 49:219-229
|
[13] |
Abdul W A, Kral M V. 3D analysis of creep voids in hydrogen reformer tubes [J].Mater. Sci. Eng. A, 2005, 412:222-229
|
[14] |
Abdul W A, Hutchinsonb C R, Kral M V. A three-dimensional characterization of creep void formation in hydrogen reformer tubes [J]. Scripta. Mater.,2006,55:69-73
|
[15] |
Ribeiro A F, de Almeida L H, Dos Santos D S, Fruchart D, Bobrovnitchii G S. Microstructural modifications induced by hydrogen in a heat resistant steel type HP-45 with Nb and Ti additions[J]. J. Alloys. Compd.,2003, 356-357:693-696
|
[16] |
Aydin I, Buehler H E, Rahmel A. Precipitation in the heat resistant nickel-base cast alloys G-NiCr 28 W and G-NiCr 50Nb [J]. Arch. Eisenhuettenwes,1983, 54(11):461-466
|
[17] |
Chen Nianjin(陈年金). Life prediction of interaction between creep and fatigue in high temperature[D].Hangzhou: Zhejiang University of Technology,2006
|
[18] |
Kong Xiangjun(孔祥军),Tao Sida(陶思达).The safety assessment and residual life prediction of furnace tubes [J].Journal of Petrochemical Universities(石油化工高等学校学报),2011,24(4):88-90, 94
|
[19] |
Wang Min(王敏).Cause analysis and control measures that affect the life of reformer tubes [J].Fertilizer Design(化肥设计),2008,46(4):48-49
|